PA66 FE3071 NC010 中粘度,注塑和擠出級(jí) 相關(guān)信息由 東莞市中嘉塑膠原料有限公司提供。如需了解更詳細(xì)的 PA66 FE3071 NC010 中粘度,注塑和擠出級(jí) 的信息,請(qǐng)點(diǎn)擊 http://www.nciecn.com/b2b/yizhanlin10.html 查看 東莞市中嘉塑膠原料有限公司 的詳細(xì)聯(lián)系方式。
PA66 FE3071 NC010 中粘度,注塑和擠出級(jí)
Zytel® FE3071 NC010 | PA66 NYLON RESIN
Regional Availability
North America, South and Central America
Processing
Injection Moulding, Film Extrusion, Profile Extrusion, Sheet Extrusion, Other Extrusion, Coatable, Casting
Delivery form
Pellets
Product Text
Common features of Zytel® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness and toughness, good high temperature performance, good electrical and flammability properties, good abrasion and chemical resistance. In addition, Zytel® nylon resins are available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses. Zytel® nylon resin, including most flame retardant grades, offer the ability to be coloured.
The good melt stability of Zytel® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.
Zytel® nylon resin typically is used in demanding applications in the automotive, furniture, domestic appliances, sporting goods and construction industry.
Zytel® FE3071 NC010 is an intermediate viscosity polyamde 66 resin for injection moulding and extrusion.
Injection molding
PREPROCESSING
Drying recommended = Yes, if moisture content of resin exceeds recommended level
Drying temperature = 80℃
Drying time, dehumidified dryer = 2-4 h
Processing moisture content = <0.05 %
PROCESSING
Melt temperature optimum = 290℃
Melt temperature range = 280-300℃
Mould temperature optimum = 70℃
Mould temperature range = 50-90℃
PROPERTIES
Mechanical properties |
dry / cond |
Unit |
Test Standard |
Tensile Modulus |
3100 / - |
MPa |
ISO 527-1/-2 |
Yield stress |
82 / - |
MPa |
ISO 527-1/-2 |
Yield strain |
4 / - |
% |
ISO 527-1/-2 |
Nominal strain at break |
35 / - |
% |
ISO 527-1/-2 |
Charpy notched impact strength,23℃ |
6 / - |
kJ/m2 |
ISO 179/1eA |
Thermal properties |
dry / cond |
Unit |
Test Standard |
Melting temperature,10℃/min |
262 / * |
℃ |
ISO 11357-1/-3 |
Temp. of deflection under load,1.8 MPa |
70 / * |
℃ |
ISO 75-1/-2 |
Temp. of deflection under load,0.45 MPa |
200 / * |
℃ |
ISO 75-1/-2 |
Other properties |
dry / cond |
Unit |
Test Standard |
Density |
1140 / - |
kg/m3 |